最近我發了一批4800TEX的紗到國外,外方反映以下問題: 紗有很多斷頭,在拉擠過程中在機器里形成很多小團,使拉擠不能繼續.請看原文:<p>On your E glass we can see some broken fibers before going into the machine. When the fiber enter into the machine these small broken thread mixed together and stop the machine creating a lot of problems.<p>拉擠用的紗到底有什么特別的要求呢?望高手指點!